How do I fix these strings?

Posted by davidf01 
How do I fix these strings?
October 08, 2015 03:46PM
I keep getting these stringy things when I print. I'm printing with a delta 2020 and slicer.
I have the PLA temperature at 195. I have set the retraction length to 3mm and the speed to 60 mm/sec.
What is better to adjust more the temp or retraction?

String picture:
Attachments:
open | download - Strings.jpg (410.4 KB)
Re: How do I fix these strings?
October 08, 2015 05:17PM
I suggest using more retraction to eliminate the blobbing, and a lower temperature after the first layer to reduce stringing. The amount of retraction you need depends on the Bowden tube length. I find I need 4 or 5mm retraction for a 350mm tube, and 8mm for a 600mm tube. I reduce temperature to 185C or 190C after the first layer. Somer people say that a slower retraction speed reduces stringing.

Edited 1 time(s). Last edit at 10/08/2015 05:18PM by dc42.



Large delta printer [miscsolutions.wordpress.com], E3D tool changer, Robotdigg SCARA printer, Crane Quad and Ormerod

Disclosure: I design Duet electronics and work on RepRapFirmware, [duet3d.com].
Re: How do I fix these strings?
October 12, 2015 02:56AM
Also the lower layers look over extruded; fixing that might help with stringing on the upper layers.