Hi everyone,
can anyone help to fix this issue?
It is a 3mm thick, 5cm tall and 15cm long rectangle and as you can see, there are two massive curling on opposite sides, separating the the layers more or less in the middle of the print.
Parameters:
1.75 ABS
225C
90C heated bed
Tried lowering speed from 60mm/s to 30mm/s
fan is on.
I believe if use bevel corners and increase the bed temperature, it might help to keep things on track. Makes sense?
Cheers,
Franklin Dattein