Hi guys,
I've a Prusa i3 with 0.4mm nozzle and a PEI sheet on the heated bed. The first layer is sticking well, but the first few additional layers seem to be way off (see attached picture).
I'm using Slic3r with layer height 0.3mm (first and others), 215° head temperature for the fist layer (PLA), 200° for additional and bed temperature of 70°.
Does anyone have an idea what the cause could be?
Thanks!