Hi I have an issue my prusa i3 was totally fine on long prints with ABS.
Now I have got some PLA and cant print long print keep clogging.
I have E3D head and separate nozzle for PLA but that not seam to help much.
I have fan 100% on to extruder heat sink.
How can I prevent this I got print to do that takes 7.30Hours but cant get past 4 hours.
Temp used 180 first layer then 175 printed fine then stopped but part felt like not heat enough.
Boosted tems to 200 ist layer then 195 but got more printed then first try and part felt much better strength wise but nozzle clogged .
How can I get rid off this problem?
PS:
ABS was printed on 260 1st layer then 255 prints so hard so nice no cracks between layers.
Regards